Тезис
ПредпросмотрISO/TR 17641-3:2005 outlines the test methods and procedures for carrying out externally loaded tests to assess susceptibility to hot cracking.
The following tests are described:
- Hot tensile tests
- Varestraint and Transvarestraint test
- Flat tensile test.
The above tests can provide information about the hot cracking sensitivity of parent materials, weld metals and weldments. Assessment is based upon the measurement of the "brittle temperature range" (BTR) where hot cracks occur.
This document applies primarily to austenitic stainless steels, nickel-, nickel-base and nickel-copper alloys, weldments and welding consumables. However, the principles can be extended to other materials such as aluminium alloys and high-strength steels.
-
Текущий статус: PublishedДата публикации: 2005-03
-
Версия: 1
-
- ICS :
- 25.160.40 Welded joints and welds
Приобрести данный стандарт
Формат | Язык | |
---|---|---|
std 1 92 | ||
std 2 92 | Бумажный |
- CHF92
Жизненный цикл
-
Сейчас
PublishedISO/TR 17641-3:2005
Стандарт, который пересматривается каждые 5 лет
Этап: 90.93 (Подтверждено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00
Появились вопросы?
Ознакомьтесь с FAQ
Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)
Будьте в курсе актуальных новостей ИСО
Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах.